HCF
Fire-protection coatings

HCF Non-intumescent protection for structural steel

A spray-applied passive protection material based on cement, vermiculite and mineral components, for interior and exterior steel columns, beams and frames.

HCF建筑应用HCF建筑应用

HCF建筑应用

Material & applications

Product designation

GT-WSF-Fp3.00-Chnitherm HCF · Exterior non-intumescent fire-protection coating for steel

Mineral passive fire protection

HCF combines high-performance cement, vermiculite and mineral components in a spray-applied protective layer for steel columns, beams and frames. Applications include interior and exterior high-rise, industrial, marine, petrochemical, tunnel, metro and underground steelwork. Specify member geometry, thickness and fire exposure together.

Material and finish

The mineral system does not require added emulsion adhesive and contains no reinforcing fibres. Spray application can be followed by surface levelling. Mesh, passes and subsequent decoration depend on the member, substrate and design thickness.

Technical data

Technical performance

Selection data; fire performance depends on the specified member and thickness.
PropertyCriteriaPerformance
Condition after mixingThick fluid without lumpsMeets requirement
Surface drying≤24 h5 h
Initial drying crack resistanceGenerally no cracks; 1–3 cracks if present, width ≤1 mmNo cracks
Bond strength≥0.05 MPa (≥1044 psf)0.31 MPa (6474.5 psf)
Compressive strength≥0.5 MPa (≥10443 psf)2.12 MPa (44277 psf)
Dry density≤650 kg/m³500 kg/m³
Thermal conductivity≤0.116 W/(m·K)≤0.078 W/(m·K)
Water resistance≥24 h24 h
pH≥7Approx. 12

Application & system

Recommended steel system

Prepare the steel, then apply Primer AK2 zinc-phosphate primer, Primer EP61 epoxy intermediate and HCF. Verify adhesion, compatibility and drying; repair corrosion and mechanical damage.

Mixing and spraying

Add water before powder and mix mechanically at low speed until uniform. Use within 4 hours while maintaining agitation. Confirm the water quantity for the application specification. Use a screw, squeeze or mortar pump with compressed air and a mortar spray head, plus pressure-resistant, abrasion-resistant steel-reinforced hose.

Application & packaging

PropertyRequirement / data
SurfacePrepare steel for corrosion protection; clean, dry and free from debris; check primer compatibility
MixingWater first, then powder; low-speed mechanical mixing; use within 4 h with continuous agitation
EquipmentScrew, squeeze or mortar pump; compressed air and mortar spray head
HosePressure-resistant, abrasion-resistant, steel-reinforced
Pump flow7–35 L/min
Auxiliary air0.3–0.4 MPa; 0.4 m³/min
DryingSurface 5 h; through dry 7 days
RecoatMinimum 16 h; check surface condition after extended intervals
Weather5–40°C; avoid wind and rain; protect during drying
Packaging & colour25 kg net; grey-white

Drying & curing

Drying and recoat

Surface dry approximately 5 hours; through dry approximately 7 days. Minimum recoat interval 16 hours. Check actual material condition before further application; surface drying alone does not establish internal drying.

Conditions & precautions

Weather and technical specification

Apply at 5–40°C and avoid high winds and rain. Protect during drying. Evaluate the specified system against the applicable GB14907, EN1363-1 / ISO834, BS476-21, ASTM E119 / UL263 or DIN4102 conditions. Hydrocarbon and tunnel fire exposures require separate assessment; standards are not universal system certifications.

Documents & specification support

Specify for your project.

Share the application, substrate, area and performance requirements to discuss a coordinated system.