UH-Mortar Thermal and acoustic mineral plaster
A mineral plaster combining high-performance cement and insulating minerals, for thermal, acoustic and finish-support functions on walls, ceilings and building substrates. For thermal insulating and sound absorbing mortar projects, discuss the substrate, compatible materials and application conditions with our factory.
Material & applications
Thermal and acoustic mineral plaster
High-performance cement and insulating minerals form a layered material with air spaces that influence heat transfer. Controlled drying coordinates internal stress, stability and the final finish. Applications include walls, ceilings and suitable building substrates in high-rise, industrial, marine, tunnel and underground environments.
Coordinated functions
Specify thickness, substrate, finish and loads together. Floor or tile applications require separate adhesion and load review. Sound absorption coefficients cannot be converted directly into wall sound-insulation decibels.
Thermal and acoustic layer concept
Tunnel application
High-rise application
Technical data
Material technical properties
| Property | Method | Performance |
|---|---|---|
| Density | ASTM E60 | 680 kg/m³ |
| Bond strength | ASTM E736 | 188545 N/m² (0.2 MPa) |
| Compressive strength | ASTM E761 | 2.5 MPa |
| Corrosion | ASTM E937 | Non-corrosive to steel |
| Impact resistance | ASTM E760 | No cracking or breakage |
| Deflection | ASTM E759 | No rupture or delamination |
| Fungal growth | ASTM G21 | No growth in 60 days |
| Combustibility | BS476 part4 | Non-combustible material |
| Flame spread & smoke | BS476 part6 | Class 0 |
| Thermal conductivity | BS874 | 0.09 W/(m·K) |
| Dust erosion | ASTM E859 | Less than 0.001 g/ft² total in 24 h |
Wall-material thermal data
| Material | Conductivity W/(m·K) | Density kg/m³ |
|---|---|---|
| Mineral plaster | 0.09 | 700 |
| Aerated concrete | 0.21 | 600 |
| Expanded-clay concrete | 0.77 | 1500 |
| Brickwork | 0.81 | 1800 |
| Mixed mortar | 0.87 | 1700 |
| Cement mortar | 0.93 | 1800 |
| Concrete | 1.52 | 2400 |
| Reinforced concrete | 1.74 | 2500 |
Sound absorption by frequency
| Frequency Hz | Octave-band absorption coefficient α |
|---|---|
| 125 | 0.15 |
| 250 | 0.37 |
| 500 | 0.44 |
| 1000 | 0.64 |
| 2000 | 0.76 |
| 4000 | 0.95 |
Durability evaluation
| Property | Conditions | Result |
|---|---|---|
| Bond strength / MPa | ≥0.04 | 0.31 |
| Compressive strength / MPa | ≥0.5 | 2.12 |
| Heat exposure | 720 h without delamination, detachment, hollowing or cracks; insulation-efficiency decline ≤35% | Appearance meets criteria; decline 9.7% |
| Humid heat | 504 h without delamination/detachment; efficiency decline ≤35% | Appearance meets criteria; decline 3.2% |
| Freeze-thaw | 15 cycles without cracking, detachment or blistering; efficiency decline ≤35% | Appearance meets criteria; decline 11.3% |
| Acid resistance | 360 h without delamination, detachment or cracks; efficiency decline ≤35% | Appearance meets criteria; decline 5.6% |
| Alkali resistance | 360 h without delamination, detachment or cracks; efficiency decline ≤35% | Appearance meets criteria; decline 4.0% |
| Salt-spray corrosion | 30 cycles without blistering, deterioration or softening; efficiency decline ≤35% | Appearance meets criteria; decline 8.1% |
| UV irradiation | 60 cycles without delamination, cracking or chalking; efficiency decline ≤35% | Appearance meets criteria; decline 8.9% |
Application & system
System and mixing
Prepare and seal the substrate, apply UH-Mortar, then the compatible decorative or functional finish. Keep the base clean and dry. Add water first, mix slowly, use within 4 hours and keep agitating. Confirm the water quantity for the application. Use a screw, squeeze or mortar pump, compressed air and steel-reinforced pressure/abrasion-resistant hose.
Application, packaging & storage
| Property | Requirement / data |
|---|---|
| Substrate | Prepare to applicable requirements; clean, dry and free from debris |
| Mixing | Water first, low-speed mixing; use within 4 h with continued agitation |
| Spray equipment | Screw/squeeze/mortar pump, compressed air, spray head and steel-reinforced pressure/abrasion-resistant hose |
| Flow | 7–35 L/min |
| Air | 0.3–0.4 MPa; 0.4 m³/min |
| Drying | Surface 3 h; through dry 7 days |
| Recoat | Minimum 16 h; check surface after extended intervals |
| Weather | 5–40°C; avoid wind/rain and protect during drying |
| Storage | Dry at 20°C, protected from light and water; 6 months |
| Packaging & colour | 25 kg net; grey-white |
Drying & curing
Drying and storage
Surface dry approximately 3 hours; through dry approximately 7 days; minimum recoat 16 hours. Check actual drying before the next operation. Grey-white material, 25 kg packaging; store dry at 20°C, away from light and water, for 6 months.
Conditions & precautions
Conditions and interpretation
Apply at 5–40°C, avoiding wind and rain; protect while drying. Thermal, acoustic, mechanical and durability properties require separate evaluation. The technical-property and performance-evaluation tables do not represent one interchangeable specimen. NRC is 0.55; absorption is shown across 125–4000 Hz, with actual behaviour dependent on thickness and mounting. Fire performance must be matched to the specified assembly and applicable test documents.
Documents & specification support
Specify for your project.
Share the application, substrate, area and performance requirements to discuss a coordinated system.